Freudenberg-NOK Part Number 58652
|
|
|
|
|
|
|
| Value |
Tolerance |
| Thickness |
.020" |
+/- .002" |
| Width |
1.00" |
+/- .020" |
| Length |
60 ft. |
+/- 6.00" |
| Tape Colour |
Red / Orange |
N/A |
| Guideline Colour |
N/A |
N/A |
| Value |
Specification |
| Tensile Strength (lbs/inch.) |
56 |
40 lbs/inch. Min |
| Elongation (%) |
25% |
15 % min. |
| Inclined Mandrel Tack Test (inch.) |
0.25 |
ASTM D2148 |
| Bond Strength (1 inch. width, pounds) |
5.5 |
1.0 lb/inch. min. |
| Dielectric Strength (Volts/mil) |
575 |
500 Min. ASTM D149 |
| * Note: This product meets the physical requirements outlined in MIL standard with added high heat resistant properties. |
| Reinforcement Material |
Sinusoidal Glass Yarn |
| Interleave Material |
.002" thk. Mylar |
| Product Operating Temperature |
-40 Deg. F to +600 Deg. F |
| Product Shelf Life |
One Year |
| Note: Shelf life is defined as the duration of time for which the product will meet the physical requirements outlined above. |
| It does not guarantee the product's usefulness in all applications. |
| Value |
Test Method |
| Tensile Strength (PSI) |
1460 |
ASTM D412 |
| Elongation (%) |
450 |
ASTM D412 |
| Tear Strength (lb/in) |
146 |
ASTM D624 Die B |
| Durometer, Shore A Points |
55 |
ASTM D2240 |
| Flame Test Method |
FAA 60 Sec. Vertical |
| Value |
Tolerance |
| Flame Time (seconds) |
N/A |
N/A |
| Glow Time (seconds) |
N/A |
15 sec. Max |
| Char Length (inches) |
N/A |
6" Max. |
| Fuel Test Information |
Value |
Test Method |
| Volume Change After 24hr Immersion @ 73F |
N/A |
ASTM D471 Ref. Fuel C |
| Hardness Change After 24hr Immersion @ 73F |
N/A |
ASTM D471 Ref. Fuel C |
| Elongation Change After 24hr Immersion @ 73F |
N/A |
ASTM D471 Ref. Fuel C |
| Tensile Change After 24hr Immersion @ 73F |
N/A |
ASTM D471 Ref. Fuel C |
|
| The data presented in this document represents typical values for the production material. |
| This data should not be used to write, or in place of, material specifications. |
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|